ASME STP PT 087 2018
$98.04
ASME STP PT 087 Yield Strength Values up to Maximum Temperature Design
Published By | Publication Date | Number of Pages |
ASME | 2018 | 102 |
Yield Strength Values up to Maximum Temperature Design. Publisher: ASME Standards Technology LLC Publish Date: 2018 Pages: 102 Language: English ISBN: 9780791872420
PDF Catalog
PDF Pages | PDF Title |
---|---|
9 | Foreword |
10 | Abstract |
11 | Abbreviations and Acronyms |
12 | 1 INTRODUCTION |
16 | 2 STEELS 2.1 S20910 / XM-19/ 22Cr-13Ni-5Mn up to 1200 F |
19 | 2.2 S30400/ 304/ 18Cr-8Ni up to 1500 F |
22 | 2.3 S30403/ 304L/18Cr-8Ni up to 1200 F |
25 | 2.4 S30908/ 309 S/ 23Cr-12Ni up to 1500 F |
28 | 2.5 S31008/ 310 S/ 25Cr-20Ni up to 1500 F |
31 | 2.6 S31600/SS 316/ 16Cr-12Ni-2Mo up to 1500 F |
33 | 2.7 S31603/ 316L/ 16Cr-12Ni-2Mo up to 1200 F |
35 | 2.8 S31635/ 316Ti/16Cr-12Ni-2Mo-Ti up to 1500 F |
38 | 2.9 S31700/ SS317/and S31703/SS317 L/ 18Cr-13Ni-3Mo up to 1500 F (1200 F) |
39 | 2.10 S32100/ SS321/ 18Cr-10Ni-Ti up to 1500 F |
42 | 2.11 S34700/ SS347 and S34800/ SS348/ 18Cr-10Ni-Cb up to 1500 F |
45 | 3 COPPER 3.1 C23000 / Cu 230 / 85 Cu-15 Zn up to 500 F |
46 | 3.2 C28000 / Cu 280 / 59 Cu-40Zn-0.07Fe-0.3Pb up to 500 F |
48 | 3.3 C36500 / Cu 365 / 60Cu-39.4 Zn-0.6 Pb |
49 | 3.4 C44300 / Cu 443 C44400 / Cu 444 C44500 / Cu 445 up to 500 F |
52 | 3.5 C46400 / Cu 464 C46500 / Cu-465 up to 500 F |
53 | 3.6 C64200 / Cu 642 / 91.2 Cu, 7.0 Al, 1.8 Si up to 500 F |
55 | 3.7 C68700 / Cu 687 / 77.5 Cu, 20.5 Zn, 2.0 Al, 0.1 As up to 500 F |
57 | 3.8 C70400 / Cu 704 / 92.4 Cu, 5.5 Ni, 1.5 Fe, 0.6 Mn up to 500 F |
58 | 3.9 C71000 / Cu 710 / 79 Cu, 21 Ni up to 700 F |
60 | 4 NICKEL 4.1 N02201 / Ni 201 up to 1200 F |
63 | 4.2 N06002 / Ni X up to 1650 F |
66 | 4.3 N06022 up to 1250 F |
69 | 4.4 N06600 / Ni 600 up to 1200 F 4.5 Annealed |
72 | 4.6 Hot Worked |
74 | 4.7 Seamless Pipe |
76 | 4.8 N06625 / Ni 625 SA up to 1600 F |
79 | 4.9 N06625 / Ni 625 Ann up to 1200 F |
82 | 4.10 N08330 / Ni 330 up to 1650 F |
85 | 4.11 N08800 / Ni 800 up to 1500 F |
88 | 4.12 N08810 / Ni 800H and N08811 / Ni 811 up to 1650 F |
91 | 4.13 N10276 / Ni C276 up to 1500 F |
94 | 4.14 N10003 / Ni N / Hastelloy N up to 1500 F |
97 | Appendix A |