Shopping Cart

No products in the cart.

ASTM-A667 2012

$35.75

A667/A667M-87(2012) Standard Specification for Centrifugally Cast Dual Metal (Gray and White Cast Iron) Cylinders

Published By Publication Date Number of Pages
ASTM 2012 2
Guaranteed Safe Checkout
Categories: ,

If you have any questions, feel free to reach out to our online customer service team by clicking on the bottom right corner. We’re here to assist you 24/7.
Email:[email protected]

ASTM A667/A667M-87-Reapproved2012

Historical Standard: Standard Specification for Centrifugally Cast Dual Metal (Gray and White Cast Iron) Cylinders

ASTM A667/A667M

Scope

1.1 This specification2 covers centrifugally cast cylinders with an outer layer of white cast iron and the remainder of the material of gray cast iron. These castings are suitable for pressure containing parts the design strength of which is based on the gray iron portion of the cylinder. These castings are suitable for service at temperatures up to 450°F [230°C].

1.2 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.

1.3 The following safety hazards caveat pertains only to the test method portion, Section 8, of this specification: This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.