ASTM-D4671:2010 Edition
$35.75
D4671-05(2010)e1 Standard Test Method for Polyurethane Raw Materials Determination of Unsaturation of Polyols
Published By | Publication Date | Number of Pages |
ASTM | 2010 | 4 |
1.1 These test methods measure unsaturation in polyether polyols. (See Note 1.)
1.1.1 Test Method A, High-Volume Reagent Method Uses about 50 mL of 0.1 M mercuric acetate reagent in methanol and 15 g or more of sample. These test methods use an indicator for colorimetric determination of an end point. It is recommended for polyols with low values (below 0.01 millequivalents per gram (meq/g)) of unsaturation where large sample sizes are required.
1.1.2 Test Method B, Low-Volume Reagent Method Uses 2 mL of ca. 0.05 M mercuric acetate reagent in methanol and about 1 g of sample or less. These test methods use a potentiometric determination of an end point.
1.2 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.
1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Note 1There is no known ISO equivalent to this standard.
PDF Catalog
PDF Pages | PDF Title |
---|---|
1 | Scope Referenced Documents Terminology Summary of Test Method Significance and Use Interferences |
2 | Apparatus Reagents Procedure Calculation Precision and Bias Apparatus |
3 | Reagents Procedure Calculation Report Precision and Bias TABLE 1 |
4 | Keywords TABLE 2 |