{"id":334055,"date":"2024-10-19T23:17:20","date_gmt":"2024-10-19T23:17:20","guid":{"rendered":"https:\/\/pdfstandards.shop\/product\/uncategorized\/bsi-16-30339916-dc\/"},"modified":"2024-10-25T22:14:48","modified_gmt":"2024-10-25T22:14:48","slug":"bsi-16-30339916-dc","status":"publish","type":"product","link":"https:\/\/pdfstandards.shop\/product\/publishers\/bsi\/bsi-16-30339916-dc\/","title":{"rendered":"BSI 16\/30339916 DC"},"content":{"rendered":"
PDF Pages<\/th>\n | PDF Title<\/th>\n<\/tr>\n | ||||||
---|---|---|---|---|---|---|---|
1<\/td>\n | 30339916 <\/td>\n<\/tr>\n | ||||||
3<\/td>\n | 2133_NWP 02-03-2016 <\/td>\n<\/tr>\n | ||||||
6<\/td>\n | 1 Scope 2 Normative references 3 Purpose of process <\/td>\n<\/tr>\n | ||||||
7<\/td>\n | 4 Limitations of process use 5 Terms and definitions 6 Coating thickness 7 Symbols 8 Information for the processor <\/td>\n<\/tr>\n | ||||||
8<\/td>\n | 9 Condition of parts prior to the treatment 10 Process schedule 10.1 Covering 10.2 Surface pre-treatment 10.3 Nickel strike 10.4 Cadmium plating <\/td>\n<\/tr>\n | ||||||
9<\/td>\n | 11 Post-treatment 11.1 De-embrittlement 11.2 Conversion 12 Removal of the plating 13 Required characteristics 13.1 Appearance <\/td>\n<\/tr>\n | ||||||
10<\/td>\n | 13.2 Adhesion 13.3 Coating thickness 13.4 Hydrogen embrittlement of steels 13.5 Corrosion resistance 14 Test methods 14.1 For process approval 14.1.1 Appearance 14.1.2 Adhesion 14.1.3 Coating thickness <\/td>\n<\/tr>\n | ||||||
11<\/td>\n | 14.1.4 Hydrogen embrittlement 14.1.5 Corrosion resistance 14.2 For acceptance of parts 14.2.1 Appearance 14.2.2 Adhesion (if agreed) 14.2.3 Coating thickness 15 Quality assurance 15.1 Approval of the processor 15.2 Process approval <\/td>\n<\/tr>\n | ||||||
12<\/td>\n | 15.3 Acceptance 15.4 Reprocessing 16 Designation <\/td>\n<\/tr>\n<\/table>\n","protected":false},"excerpt":{"rendered":" BS EN 2133. Aerospace series. Cadmium plating of steels with specified tensile strength \u2264 1 450 MPa, copper, copper alloys and nickel alloys<\/b><\/p>\n |